Assessing wear: tables per rope construction
Assessment tables in green, amber and red for 8-strand rope (including PP/PE mooring lines), 12-strand rope and core-cover: what you see, what it means and what to do.
How you assess wear depends on the construction. These tables help the crew and the qualified person decide quickly and consistently. When in doubt, safety always comes first.
- Serviceable no action needed, or maintenance by a qualified person to extend service life.
- Limited use damage visible; remove the cause, repair or resplice, and monitor the line closely.
- Immediate action cut out the damaged section and resplice, or retire the whole line and dispose of it properly.
8-strand rope (including PP/PE mooring lines such as Tipto)
In 8-strand rope all strands carry load, so you see damage directly on the load-bearing fibres. Typical for mooring lines in polypropylene, polyolefin and blends.
| What you see | Verdict | Action |
|---|---|---|
| As new, shiny surface | Serviceable | None |
| Light surface fuzz | Serviceable | None |
| Matt surface, more fuzz, construction still clearly visible | Limited use | Limited to no more than 4× rope diameter? Find the cause at the fittings and remove it. |
| Even more fuzz, longer protruding fibres, construction still visible | Limited use | As above; inspect more often. |
| Fully covered in fuzz, whole yarns broken, structure no longer recognisable | Immediate action | Local (max. 4× diameter): cut out and resplice. Otherwise retire the whole line. |
| Externally compressed | Serviceable | Assess further for wear and cut yarns. |
| Soiled | Serviceable | Rinse with lukewarm running water if needed. |
| Pulled yarns or strand | Limited use | Work them back into the structure. |
| Less than 10% of yarns cut | Limited use | Work yarns back in; inspect more often. |
| Twist, fewer than 4 turns per metre | Limited use | Turn the rope back to its original state. |
| Heat damage or fusing | Immediate action | Shorter than 4× diameter: cut out and resplice. Otherwise retire. |
| One strand completely cut | Immediate action | Retire, or cut out and resplice. |
| Several strands partly cut, more than 10% of yarns | Immediate action | Retire, or cut out and resplice. |
| Label damaged or illegible | Immediate action | Have the label renewed; no use without identification. |
12-strand rope (HMPE and modern mooring lines)
In 12-strand rope without a cover every strand carries load. Because every strand is visible, inspection is relatively straightforward.
| What you see | Verdict | Action |
|---|---|---|
| Light fuzz, construction clearly visible | Serviceable | None |
| Glazed or shiny hard areas | Limited use | Possible heat: have a qualified person assess. |
| Fibre dust between strands when opened | Limited use | Internal wear: rinse, inspect more often. Lots of dust: retire. |
| Pulled strand | Limited use | Work the strand back in. |
| Less than 10% of yarns cut | Limited use | Inspect more often; cut out if needed. |
| Twist | Limited use | Turn back; watch the longitudinal marking. |
| Heat damage, fusing, hard areas | Immediate action | Cut out and resplice, or retire. |
| One strand cut or more than 10% of yarns | Immediate action | Cut out and resplice, or retire. |
| Damage to the splice area | Immediate action | Resplice by a professional, or retire. |
Core and cover (core carries the load)
Here the cover protects the load-bearing core. As long as the core is undamaged, cover damage can often be repaired. If the core shows or is itself damaged, immediate action is required.
| What you see | Verdict | Action |
|---|---|---|
| Light fuzz on the cover | Serviceable | None |
| Cover matt and heavily fuzzed, but intact | Limited use | Find the cause at the fittings; inspect more often. |
| Holes or cut in the cover, core not visible | Limited use | Have the cover repaired by a professional. |
| Cover sliding over the core (bunching) | Limited use | Have it assessed; cover repair may be possible. |
| Core visible through the cover | Immediate action | Have it assessed straight away; usually cut out or retire. |
| Core damaged or fused | Immediate action | Retire, or cut out and resplice. |
there are visible effects of a heavy shock load, major heat damage, damage that cannot be localised, or if the origin and certificate of the line can no longer be established.